Fig. 2: Given equal deposition duration and crucible temperature, adsorption of precursor 1 onto the Au(111) surface and subsequent growth into polymers is dictated by substrate temperature during deposition.

All samples were created with identical deposition durations and crucible temperatures, with the only variation being in substrate temperature during deposition. a, c, e Large-scale and b, d, f small-scale scans of polymer assemblies from depositions performed at 22, 100, and 180 °C substrate temperatures, respectively. The green circle in b indicates a bright spot due to iodine that remains on the surface. Scan parameters: a -1.95 V, 30 pA; b 1.9 V, 10 pA; c -0.75 V, 30 pA; d -0.25 V, 10 pA; e, f -1.5 V, 15 pA.