Fig. 7: Schematic of the electrode fabrication process with corresponding images of the electrospun mat at each stage.
From: Acute deformation characteristics of standard and flexible lithium-ion battery electrodes

Step 1: Co-electrospinning and electrospraying of PAN/DMF/MWCNT and LFP/DMF/PAN solutions. Step 2: Pre-oxidation at 280 °C for 1 h (1 °C/min ramp-up, 5 °C/min ramp-down). Step 3: Carbonization at 550 °C for 5 h (1 °C/min ramp-up, 5 °C/min ramp-down).