Table 2 Tensile results
From: Localised control of phase formation in a high-carbon low alloy steel by laser powder bed fusion
Sample | Fracture stress (MPa) | Fracture strain (%) |
|---|---|---|
Banded microstructure print | 905.7 ± 55.0 | 1.4 ± 0.7 |