A two-step spray coating process (first step: 20 cycles of spray coating at 110 °C with 40 s intervals; second step: 180 cycles of spray coating at 130 °C with 20 s intervals) was employed to a produce large-area, compact, and thick Cs3Bi2I9 perovskite film for the application of direct X-ray detectors. The fabricated device achieved a large active area of 150 mm2, a sensitivity of 127.23 μC Gyair−1 cm−2, a detection limit of 7.4 μGyairs−1, and durability after long-term X-ray pulse irradiation.
- Yen-Ting Chen
- Zi-Xiang Wen
- Peter Chen