Fig. 3: XRD patterns of mixed Cu-Ti3AlC2 powders and the UAHP prepared Cu-Ti3AlC2 composites.
From: Ultrasonic-assisted hot-press sintering of Cu-Ti₃AlC₂ composites

a The XRD pattern of mixed Cu-30 vol.% Ti3AlC2 powers. b XRD patterns of as-prepared Cu-(5–30) vol.% Ti₃AlC₂ composites. c The magnified Cu (111) and Cu (200) peaks in the XRD patterns of different Cu-Ti3AlC2 composites.